In this study the aim is to determine the percentage of glass replacement, resulting in optimal compressive strength.Concrete nominal mix of M20 with different percentages of Glass power has been evaluated as per IS 2386(part IV) and IS 383. Waste glass powder was replace with fine aggregate in various percentages such as 5%,10%,15%,20%,25%,30%,35%,40%,45%, and 50%. Reference concrete mix is also made for comparative reasons.
Sudhanshu Kumar | Dr. Bharat Nagar"Effects of Waste Glass Powder on Compressive Strength of Concrete"
Published in International Journal of Trend in Scientific Research and Development (ijtsrd), ISSN: 2456-6470, Volume-1 | Issue-4 , June 2017,
Paper URL: http://www.ijtsrd.com/papers/ijtsrd136.pdf
Direct URL: http://www.ijtsrd.com/engineering/civil-engineering/136/effects-of-waste-glass-powder-on-compressive-strength-of-concrete/sudhanshu-kumar